Blog on cast iron moulding

Technical articles on cast iron, machine moulding, heat treatment and rapid prototyping from the foundry in Mosbach. Written for design and purchasing.

Engineers review a drawing for casting-friendly design
Casting designAugust 26, 2025

Casting-friendly design

Draft, parting, radii and machining datums before the drawing goes out to quote. Wall thickness stays a separate text.

Read more →
Dimensional inspection of a casting with a measuring arm
Quality & inspectionAugust 26, 2025

Casting defects and inspection

Shrink, gas, cold shut, core shift. Which test at Röth finds which fault, and what is already settled before the first flask.

Read more →
Core and pattern work on a ribbed housing
Moulding processesAugust 26, 2025

Cores and core-heavy housings

Why cores set wall, position and tightness. What a core assembly asks of the moulder, and where Röth pours that on the HWS line.

Read more →
MAGMA solidification simulation of a casting
Quality & inspectionAugust 26, 2025

Solidification simulation with MAGMA

What the run shows before the first flask: fill, shrink, gas, hardness field and stress. At Röth since 2008 when 3D data exist.

Read more →
Printed sand mould for a casting prototype
Rapid prototypingAugust 26, 2025

From prototype to series

When sand 3D printing stops and when a pattern plus HWS or Disamatic starts. Same grade, different cost, different time.

Read more →
Machine moulding compared with hand moulding
Moulding processesFebruary 17, 2025

Machine moulding and hand moulding

HWS and Disamatic in green sand: flask, mould block, lot and cores. Hand moulding of multi-tonne parts is not Mosbach.

Read more →
3D sand printing in the foundry
Rapid prototypingFebruary 15, 2025

Rapid prototyping with sand 3D printing

STP to a sand mould, no pattern. 15–25 working days, poured in GJL or GJS, then series on HWS or Disamatic.

Read more →
Heavily rusted casting
Quality & inspectionJanuary 20, 2025

Corrosion protection for cast-iron raw parts

After fettling and blasting flash rust sets in, and VCI or oil protect until machining. Lasting protection comes after cutting, not as paint from the foundry.

Read more →
Annealing furnace at work
Materials & metallurgyJanuary 10, 2025

Annealing cast iron

Stress relief, soft or pearlitic: aim and temperature belong on the same order. Graphite shape comes from the melt, not from the furnace.

Read more →
What cast iron is
Materials & metallurgyJanuary 7, 2025

Cast iron as a material

GJL damps, GJS carries tension. Röth pours both to DIN EN 1561 and 1563. The bar figure is not housing strength.

Read more →
Wall thickness of iron castings
Casting designJanuary 4, 2025

Wall thickness in iron castings

Wall thickness sets cooling and structure — 3 mm is shop practice on the moulding line, not a standard. Jumps without a radius feed the node, not the strength.

Read more →
Density of cast iron
Materials & metallurgyJanuary 3, 2025

Density of cast iron

GJL typically 7.10–7.25 g/cm³, GJS often 7.1–7.2 — guide values for piece weight and freight. Density is not acceptance and explains neither grade nor damping.

Read more →

Planning a casting?

We support you from design to series production: machine moulding, core making and materials advice.

See capabilities