SEIATSU

Air-flow squeeze moulding process of the HWS

Also called: SEIATSU process, Air-flow squeeze moulding

What is SEIATSU?

SEIATSU is an air-flow squeeze moulding process. First air flows through the moulding sand, then the squeeze follows. The aim is even compaction in the flask. At Röth the HWS moulding line works by this process. SEIATSU is a moulding process, not an alloy and not a certificate. It does not sit beside EN-GJL-250 on the drawing and not as a grade on the delivery note.

01

What it is

Squeeze alone compacts more at the top than at the bottom. The air flow loosens first and lays the sand onto the contour; the press closes after, and the sand sits more evenly on the pattern.

Even mould hardness holds the contour during the pour. Soft pockets erode. Hard edges tear on withdrawal. SEIATSU aims at the middle, not at peak hardness at any price.

The process needs flowable green sand. Bentonite and water must sit in the window. Lumpy sand does not follow the air flow into the pockets.

SEIATSU works in the flask. The frame holds the sand while air and press act. Flaskless moulding on the Disamatic compacts differently. The word does not belong there.

Air flow plus squeeze is moulding technique, not a material, not a grade, not an inspection mark. GJL or GJS is iron, SEIATSU is the HWS. The delivery note names the grade, not the air flow.

02

In the shop / at Röth

SEIATSU is the compaction of the HWS, not of the Disamatic. Flask size and piece weight 5-200 kg sit under flask moulding. The focus is core-intensive housings.

The customer notices it in more even castings in tight tolerances, not in the name on the delivery note. The grade stays GJL or GJS. The raw casting stays fettled, often blasted.

Sand testing holds moisture and strength. Without that window the air flow is no use. The sand must first flow, then hold. Lumps in the mixer are scrap before the mould.

Cores stay resol-CO₂. SEIATSU moulds the outer mould. The core sits in the flask after that. Compaction and core are neighbours, not the same. The air flow compacts sand, it does not harden a binder.

Prototypes may be printed. The series returns to the HWS with SEIATSU. MAGMA lays gating and feeders into this flask, not into a process as a brand. The print does not compact by air flow.

03

What matters in practice

Even mould hardness helps the contour. It does not replace a castable part or a clean core. An undercut without a core stays unmouldable, also after SEIATSU. The press moulds sand, not iron.

Joint, draft and sand window decide whether the contour withdraws. The air flow fills pockets. Withdrawal needs draft and plasticity.

Draft and pattern surface decide withdrawal after compaction. Hard and sticky tears. Soft and tapered holds.

Core-intensive housings use the advantage: even hardness around prints and ribs. The core stays chemical. SEIATSU only moulds the green sand around it.

  • Expect SEIATSU only on the HWS, not on the Disamatic.
  • Test the moulding material, otherwise the air flow stays useless.
  • Think core and outer mould separately.
  • Do not write SEIATSU on the drawing or the order.
  • Air flow first, squeeze after: without the first step the pocket stays soft.

04

Typical mistake

Read SEIATSU as a casting alloy or as a certificate. It is a moulding process. It does not sit beside EN-GJL-250 on the drawing.

Describe the Disamatic with SEIATSU. The mould block compacts differently. The word belongs to the HWS.

Confuse even compaction with arbitrary geometry. What does not fit the flask, nobody compacts, not even with air flow.

Ignore the moulding material and only praise the process. Bentonite, water and testing carry the hardness. The machine distributes it.

Write SEIATSU on the drawing like a heat treatment. Purchasing cannot inspect that. The moulding line runs it or not.

05

Limit

Not a plant manual. The text places the word that sits on the Röth page at the HWS. Pressures, times and nozzles stay shop data.

SEIATSU is not an offer for hand moulding, permanent mould or die casting. It is the compaction of a machine moulding line in Mosbach.

This entry does not replace a moulding check. Whether a housing holds the contour is shown by sand, core and first part.

What is delivered is iron as a raw casting. SEIATSU does not sit as a grade on the delivery note. The agreed specification does that.

No licence customer. The word places the HWS. Pressures and times stay internal. The customer orders iron, not air flow. SEIATSU stays a moulding process.

Back to the lexicon